色综合,色综合,色综合,亚洲一区二区三区久久久精品,久久久久久久久国产av http://m.owweac.cn/tr/cimentolu-karbur-hassas-ilerici-kaliplarin-kirilmasina-nedenleri%ef%bc%9f/ Tue, 31 May 2022 09:59:20 +0000 saatlik 1 https://wordpress.org/?v=6.7.2 Yazar: Tim http://m.owweac.cn/tr/cimentolu-karbur-hassas-ilerici-kaliplarin-kirilmasina-nedenleri%ef%bc%9f/#comment-10520 Tue, 31 May 2022 09:59:20 +0000 http://m.owweac.cn/?p=20728#comment-10520 Muhsin yorumuna yan?t olarak.

Hello Muhsin,
Thanks for your comment.
We would recommend low cobalt around 6-8% for carbide drawing dies and high cobalt 15-25% for carbide cold heading dies.
The density is around 13.5-14.5 g/cm^3.
If you have any inquiries, feel free to contact us at sales@meetyoucarbide.com
Best regards,
Tim

]]>
Yazar: Muhsin http://m.owweac.cn/tr/cimentolu-karbur-hassas-ilerici-kaliplarin-kirilmasina-nedenleri%ef%bc%9f/#comment-10513 Tue, 31 May 2022 07:21:13 +0000 http://m.owweac.cn/?p=20728#comment-10513 Kal?p alan?nda kullan?lmas?n? tavsiye etti?iniz karbür nedir. Yo?unluk bak?m?ndan GB ka? olmal?d?r? Not: Pres bask? esnas?nda ?ekil verdi?i malzeme pirin?’tir. Te?ekkürler

]]>